Focus on SMC cores
soft magnetic composites used on TFM
LOADING IMAGES
soft magnetic composites used on TFM

Raw material: high purity iron powder coated with insulating layer
Size (mm): 43H-28W-13H, soft magnetic composite cores are shaped according to the moulds
Density: ≥7.4g/cm³
Heat treatment temperature: about 600°C
Surface treatment: No