Raw material: high purity iron powder coated with insulating layer
Size (mm): L87-W26-W17-H23, sizes and shapes of soft magnetic composite cores can be customized
Density: about 7.4g/cm³
Heat treatment temperature: about 650°C
Surface treatment: No
Advantages Soft Magnetic Composites:
1. Less parts and assemble easily
2. High power density by 3D magnetic flux
3. Quick response,Fast and accurate drive
4. Complex shapes can be made easily, making the design more flexible
5. Lower eddy current losses at high frequencies compared with lamination steel
6. Reducing the size and the weight of the motor significantly, saving copper
7. Soft Magnetic Composite can improve the motor/engine performance, and can reduce cost obviously.
Raw material: high purity iron powder coated with insulating layer
Size (mm): L87-W26-W17-H23, sizes and shapes of soft magnetic composite cores can be customized
Density: about 7.4g/cm³
Heat treatment temperature: about 650°C
Surface treatment: No