Focus on SMC cores
generator cores using soft magnetic composites
LOADING IMAGES
generator cores using soft magnetic composites

Raw material: high purity iron powder coated with insulating layer
Size (mm): R93-R20-23H, soft magnetic composite cores are shaped according to the moulds
Density: ≥7.4g/cm³
Heat treatment temperature: about 500°C
Surface treatment: No