ABS motor cores with SMCs

Raw material: high purity iron powder coated with insulating layer
Size (mm): R33-r24-4.5h, soft magnetic composite cores are shaped according to the moulds
Density: ≥7.4g/cm³
Heat treatment temperature: about 600°C
Surface treatment: No